Surface characteristics of scots pine wood heated at high temperatures after weathering

Yükleniyor...
Küçük Resim

Tarih

2017

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Slovak Forest Products Research Inst

Erişim Hakkı

info:eu-repo/semantics/closedAccess

Özet

This study was conducted to investigate some surface properties of wood specimens of heat treated Scots pine (Pinus sylvestris L.) after weathering such as surface hardness, surface roughness, gloss, and color changes. Heat treatment of Scots pine wood was carried out by hot air in an oven for 1, 2, and 3 hours at 210, 220, and 230 degrees C. The results showed that generally surface hardness losses of heat treated Scots pine wood were lower than that of un-heated Scots pine wood after weathering. Heat treated Scots pine wood gave smooth surface after weathering. Except for heat treatment at 230 degrees C for 1 and 2 hours, heat treatment resulted in better glossiness compared to un-heated Scots pine wood after weathering. According to the test results, while heat treated Scots pine wood become lighter after weathering, un-heated wood become darken after weathering. In general, heat treated wood surface to become reddish and yellowish after weathering.

Açıklama

Anahtar Kelimeler

Scots pine, Heat treatment, Weathering, Color, Surface roughness, Surface hardness, Gloss

Kaynak

Wood Research