Accelerated weathering performance of scots pine preimpregnated with copper based chemicals before varnish coating. Part II: Coated with water based varnish

dc.authorid0000-0002-7771-6993en_US
dc.contributor.authorGündüz, Ahmet
dc.contributor.authorBaysal, Ergün
dc.contributor.authorTürkoğlu, Türkay
dc.contributor.authorKüçüktüvek, Mustafa
dc.contributor.authorAltay, Çağlar
dc.contributor.authorPeker, Hüseyin
dc.contributor.authorToker, Hilmi
dc.date.accessioned2021-01-11T09:20:44Z
dc.date.available2021-01-11T09:20:44Z
dc.date.issued2019
dc.departmentAÇÜ, Orman Fakültesien_US
dc.descriptionThis study was made use of M.Sc. Thesis by Ahmet Gunduz in Graduate School of Natural and Applied Sciences at Mugla Sitki Kocman University, Turkey. This thesis has been granted by the Mugla Sitki Kocman University Research Projects Coordination Office through Project Grant Number (16/030).en_US
dc.description.abstractThis study was designed to investigate some surface characteristics such as gloss, color, and surface hardness changes of Scots pine wood preimpregnated with some copper-based chemicals before varnish coating after accelerated weathering. While Adolit KD-5 (AD-KD 5), Wolmanit CX-8 (WCX-8), and Celcure AC-500 (CAC-500) were used as copper-based impregnation chemicals, water-based varnish (WBV) was used as a coating material. Results showed that surface hardness and gloss values of Scots pine were increased after accelerated weathering. Impregnated and WBV coated Scots pine gave better surface characteristics compared to only WBV coated Scots pine. In impregnation chemicals, while AD-KD 5 showed the most appropriate chemical, in terms of surface hardness and total color changes, CAC-500 was found the most valuable chemical in terms of gloss changes after 1000 h accelerated weathering exposure.
dc.identifier.citationGündüz, A., Baysal, E., Türkoğlu, T., Küçüktüvek, M., Altay, Ç., Peker, H. and Toker, H. (2019). Accelerated weathering performance of scots pine preimpregnated with copper based chemicals before varnish coating. Part II: Coated with water based varnish. Wood Research. 64(6), 987-998.en_US
dc.identifier.endpage998en_US
dc.identifier.issue6en_US
dc.identifier.scopusqualityQ2
dc.identifier.startpage987en_US
dc.identifier.urihttps://hdl.handle.net/11494/2537
dc.identifier.volume64en_US
dc.identifier.wosqualityQ3
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.institutionauthorPeker, Hüseyin
dc.language.isoenen_US
dc.publisherSlovak Forest Products Research Insten_US
dc.relation.ispartofWood Research
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectScots pineen_US
dc.subjectSurface propertiesen_US
dc.subjectCopper-based chemicalsen_US
dc.subjectWater-based varnishen_US
dc.subjectAccelerated weatheringen_US
dc.titleAccelerated weathering performance of scots pine preimpregnated with copper based chemicals before varnish coating. Part II: Coated with water based varnishen_US
dc.typeArticle